Originally Posted by bullfrogg0 View Post
The crystallization you see might be one of the places where I ran out of argon and struck an arc and started burning up the tungsten. Yes, that happened quite a bit cuz I was trying to get all the argon I could out of the bottles I had before moving on to the full bottle
THIS THIS THIS . is how i know your an idiot.

when you run out of argon you get Porosity because theres nothing to sheild the weld.

too much heat looks like THIS

[IMG][/IMG]

which looks like THIS



h